| Quality | Unit | UDD | UDD-G | PDD |
|---|---|---|---|---|
| The size of a primary crystal | nano | 4~6 | 4~15 | 0~12µm |
| The size of uncrushable aggregates | nano | 5~20 | 50~200 | 79 |
| Specific surface | ㎡/g | 300±30 | 400±30 | 60~120 |
| Density(pycnometric) | g/cm3 | 3.1~3.2 | 3.39 | |
| The beginning of an air oxidation (Depends on purity UDD) |
℃ | -450 | -450 | -450 |
| Temperature of the beginning of vacuum graphitization |
℃ | -1100 | -1100 | -1100 |
| Percentage of Diamond | % | 97~99 | 52~80 | 100 |
| Color | Gray | Black | Gray | |
| Shape | Bucky | Black & Thin Band | ||
| Bulk Weight | g/cm3 | 0.4~0.6 | ||
| Pore volume | cm3/g | 1.314 | ||
| Constant of crystal lattice | nano | 0.3573±0.0005 |
Remarks:
- UDD(Ultra Dispersed Diamond)
- UDD-G(Ultra Dispersed Diamond + Graphite)
- PDD(Polycrystalline Detonated Diamond Powder)
Nano Diamond Application
- Electrochemical plating metal(Cr, Ni, Zn, Cu, Au, Ag, Pt, etc.) and anodization of Aluminum and its alloy
- Lubricant oils, Lubricants, Lubricant-coolant, Greases (Antifriction, Antiwear, Lubricant, Compositions)
- Nano-diamond for PTFE(ploytetrafluoroethylene)
- Nano Diamond for Abrasive Tools
- Polymer Composite (Films, Rubber, Resin, Paint & Membranes)
- Nano-diamond for Polishing - by Microabrasive and Polished Compositions
- Nano-diamond for systems of Recording - UDD
Advantages of Nano Diamond
Increase in quality and competitiveness, i.e.
- Increase wear-resistance & high microhardness
- Increase in corrosion resistance
- Heightened abrasion resistance
- High fill-ability and low porosity.
- Heightened adhesion.
- Lowered friction coefficient.
- High electro- and thermal-insulation properties.
Increase in service life of products.
Saving in materials, energy-and labor costs.